DO YOU PREFER TO BUY ON-LINE?

Mai 14, 2019

Tiziana

Stella Welding Alloys catalogue is now available on misterworker.com

Starting today, our range of alloys and fluxes is available on Mister Worker™, an international online store that has become a point of reference for professionals in the field of maintenance, industries and building sites.
With more than 35,000 professional tools for sale, www.misterworker.com is amongst the main institutions in the Italian landscape when it comes to online B2B sales.
Ranging from Silver Brazing Alloys to Copper-Phosphorous Alloys used for Brazing, and from Fluxes to Alloys used for Welding, Mister Worker™ is provided with all our catalogue and sells it at very competitive prices, also with special offers.

Purchasing on www.misterworker.com is easy and fast: the online store is very intuitive, and you can choose amongst several payment methods available, such as credit card, PayPal, wire transfer, Sofort and many others.
Shipping costs are minimal (starting from 5,99 Euro), and the delivery time of the purchased goods is also very fast since the store ships with the best international couriers.
Also, if you have special requests and/or in need for important purchases, Mister Worker™ Customer Service will be glad to help you with technical advices and to provide you with custom quotes based on your specific needs.

Click here to access to Stella Welding Online Store on Mister Worker™

Brillen

Tiziana

Hartlote für die Herstellung von: Brillen, Brillenscharnier.
Lieferbar auch als flacher Draht:
Dicke 0,1 – 0,12 – 0,15 – 0,2 mm
Breite: 1,2 – 1,3 – 1,5 – 1,7 – 2,0 mm
Lieferbar auch als dünner Draht: Ø ab 0,3 mm

Silberhartlote

Artikel Zusammensetzung % Schmelzbereich SOL-LIQ Dichte Zugfestigkeit Normung
Ag Cu Zn Ni Mn Si Sn In °C g/cm3 kg/mm2 ISO 17672 EN 1044 AWS A5.8

Alloys

Ag40Ni 40 30 28 2 670-780 8,9 Ag 440 BAg-4
Ag40Ni/1 40 58 2 780-900 9,6 35
Anmerkungen Für Edelstahl in feuchten Umgebungen. Ag40Ni/1 ist auch für Ofenlöten geeignet.
Ag44 45 30 26 675-735 9,1 51 Ag 244 AG 203
Ag45Sn 45 27 25,5 2,5 640-680 9,2 43 Ag 145 AG 104 BAg-36
Ag49MnNi 49 16 23 4,5 7,5 680-705 8,9 55 Ag 449 AG 502 BAg-22
Anmerkungen Für Hartmetall.
Ag50Ni 50 20 28 2 660-705 9,0 45 Ag 450 BAg-24
Anmerkungen Für Edelstahl in feuchten Umgebungen.
Ag55Sn 55 21 22 2 630-660 9,4 44 Ag 155 AG 103
Ag56Sn 56 22 17 5 620-655 9,4 48 Ag 156 AG 102 BAg-7
Ag60 60 26 14 695-730 9,5 45 AG 202
Ag60Sn 60 23 14 3 620-685 9,6 48 AG 101
Ag72 72 28 780-780 10 35 Ag 272 AG 401 BAg-8
Anmerkungen Diese Legierungen sind für Ofenlöten geeignet. Ag60Sn/1 ist auch für Edelstahl in feuchten Umgebungen geeignet.

Fluxes

FLUX AG4 Allgemeine Verwendung – Sehr weit Temperaturbereich
FLUX AG7 Allgemeine Verwendung. Auch für Edelstahl
FLUX AG8 Für Edelstahl und Hartmetall – Braune Paste

Kupferphosphorlote

Artikel Zusammensetzung % Schmelzbereich SOL-LIQ Arbeitstemperatur Dichte Zugfestigkeit Normung
Ag Cu P Sn °C °C g/cm3 kg/mm2 ISO 17672 EN 1044 AWS A5.8

Alloys

Ag15CuP 15 Bal. 5 645-800 700 8,4 54 CuP 284 CP 102 BCuP-5

Fluxes

FLUX AG4 Allgemeine Verwendung – Sehr weit Temperaturbereich


SILBER -UND SCHMUCKWAREN

Tiziana

Hartlote für die Herstellung von:
Metallrahmen, Schnallen, Scharnier, Taschenverschlußen, Metallknöpfe, Kurzwaren, Silber-und Schmuckwaren, Teekessel, usw.

Hartlote

Artikel Zusammensetzung % Schmelzbereich SOL-LIQ Dichte Zugfestigkeit Normung
Ag Cu Zn Sn Si °C g/cm3 kg/mm2 ISO 17672 EN 1044 AWS A5.8

Alloys

Ag74 74 18 8 740-780 9.8 41
Ag67.5 67.5 23.5 9 700-730 9.7 47
Ag60 60 26 14 695-730 9,5 45 AG 202
Ag60Sn 60 23 14 3 620-685 9,6 48 AG 101
Ag55Sn 55 21 22 2 630-660 9,4 44 Ag 155 AG 103
Ag56Sn 56 22 17 5 620-655 9,4 48 Ag 156 AG 102 BAg-7

Fluxes

FLUX AG1 Allgemeine Verwendung
FLUX AG4 Allgemeine Verwendung – Sehr weit Temperaturbereich
FLUX AG7 Allgemeine Verwendung. Auch für Edelstahl

Weichlote

Artikel Zusammensetzung % Schmelzbereich SOL-LIQ Normung
Sn Pb Ag Cu Sb Zn Cd °C ISO 9453 EN 29453

Alloys

Ag10Sn 90 10 221-300
SnSb95/5 95 5 230-240 No. 201 S-Sn95Sb5
Ag5Sn 95 5 221-235 No. 704
Ag3,5Sn 96,5 3.5 221 No. 703 S-Sn97Ag3
SnPb60/40 60 40 183-190 No. 103 S-Sn60Pb40

Fluxes

FLUX SN1 Allgemeine Verwendung


HEIZUNG UND HANDTUCHTROCKNER

Tiziana

Hartlote für die Herstellung von:
Heizkörper, Handtuchtrockner, Thermogeräte, usw.

Messing

Artikel Zusammensetzung % Schmelzbereich SOL-LIQ Dichte Zugfestigkeit Normung
Cu Zn Ag Ni Mn Sn Si B Co P °C g/cm3 kg/mm2 ISO 17672 EN 1044 AWS A5.8

Alloys

Cu60Zn 60 Bal 0,3 875-895 8,4 40 Cu 470a CU 301
Cu59ZnSn 59 Bal 0,4 0,3 875-895 8,4 45 Cu 470 CU 302 RBCuZn-A
Cu59ZnSnMn 59 Bal 0,7 0,4 0,3 870-890 8,4 45 ~ Cu 471 ~ CU 304 ~ RBCuZn-C
Cu59ZnAg 59 Bal 1 0,1 0,1 0,1 860-890 8,4 45
Anmerkungen Messing für Hochtemperaturlöten. RoHS-konform. Lieferbar als Stäbe, umhüllte Stäbe, Drähte und Ringe. Cu59ZnAg ist für vezinkten Stahl geeignet.

Fluxes

FLUX BR1 Messinglöten
FLUX LI2 Zum Löten mit Vaporizator. Mittel-hohe Konzentration
FLUX LI3 Zum Löten mit Vaporizator. Hohe Konzentration

Kufper- und Messingpasten

Artikel Zusammensetzung % Schmelzbereich SOL-LIQ Dichte Zugfestigkeit Brinell-Härte Normung
Cu Sn P °C g/cm3 kg/mm2 HB 2,5 DIN 1733 AWS A5.7

Alloys

Cu99,9 99.9 0.05 1080 8.9 22 50 ERCu
Anmerkungen Kupferpaste für Ofenlöten.
CuSn8 Bal 8 0.1 875-1025 8.8 26 80 SG-CuSn6 ERCuSn-C
CuSn12 Bal 13 0.2 825-990 8.6 32 120 SG-CuSn12
Anmerkungen Bronzepaste für Ofenlöten.

Silberlegierungen

Artikel Zusammensetzung % Schmelzbereich SOL-LIQ Dichte Zugfestigkeit Normung
Ag Cu Zn Sn Si °C g/cm3 kg/mm2 ISO 17672 EN 1044 AWS A5.8

Alloys

Ag12 12 48 40 0,15 800-830 8,4 48 Ag 212 AG 207
Ag20 20 44 36 0,15 690-810 8,7 43 AG 206
Ag30Sn 30 36 32 2 665-755 8,8 48 Ag 130 AG 107
Ag34Sn 34 36 27,5 2,5 630-730 9 48 Ag 134 AG 106
Ag40Sn 40 30 28 2 650-710 9,1 44 Ag 140 AG 105 BAg-28
Ag45Sn 45 27 25,5 2,5 640-680 9,2 43 Ag 145 AG 104 BAg-36
Ag55Sn 55 21 22 2 630-660 9,4 44 Ag 155 AG 103
Anmerkungen Cadmium-freie und RoHS-konform. Lieferbar als Stäbe, umhüllte Stäbe, Drähte und Ringe (Abmessungen auf Anfrage).

Fluxes

FLUX AG1 Allgemeine Verwendung
FLUX AG4 Allgemeine Verwendung – Sehr weit Temperaturbereich
FLUX AG7 Allgemeine Verwendung. Auch für Edelstahl


BELEUCHTUNGSKÖRPER UND LUSTER

Tiziana

Hartlote für die Herstellung von:
Lüster, Möbelmetallzubehör, Metallkunstgegenstände, Blechmusikinstrumente, usw.

Silberlegierungen

Artikel Zusammensetzung % Schmelzbereich SOL-LIQ Dichte Zugfestigkeit Normung
Ag Cu Zn Sn Si °C g/cm3 kg/mm2 ISO 17672 EN 1044 AWS A5.8

Alloys

Ag12 12 48 40 0,15 800-830 8,4 48 Ag 212 AG 207
Ag20 20 44 36 0,15 690-810 8,7 43 AG 206
Anmerkungen RoHS-konform. Farbe Messing ähnlich.
Ag34Sn 34 36 27,5 2,5 630-730 9 48 Ag 134 AG 106
Ag40Sn 40 30 28 2 650-710 9,1 44 Ag 140 AG 105 BAg-28
Ag45Sn 45 27 25,5 2,5 640-680 9,2 43 Ag 145 AG 104 BAg-36
Ag55Sn 55 21 22 2 630-660 9,4 44 Ag 155 AG 103
Ag60Sn 60 23 14 3 620-685 9,6 48 AG 101
Anmerkungen x

Fluxes

FLUX AG1 Allgemeine Verwendung
FLUX AG4 Allgemeine Verwendung – Sehr weit Temperaturbereich
FLUX AG7 Allgemeine Verwendung. Auch für Edelstahl

Messing

Artikel Zusammensetzung % Schmelzbereich SOL-LIQ Dichte Zugfestigkeit Normung
Cu Zn Ag Ni Mn Sn Si B Co P °C g/cm3 kg/mm2 ISO 17672 EN 1044 AWS A5.8

Alloys

Cu60Zn 60 Bal 0,3 875-895 8,4 40 Cu 470a CU 301
Cu59ZnSn 59 Bal 0,4 0,3 875-895 8,4 45 Cu 470 CU 302 RBCuZn-A
Cu59ZnAg 59 Bal 1 0,1 0,1 0,1 860-890 8,4 45
Cu48ZnNi10 48 Bal 10 0,3 890-920 8,7 54 Cu 773 CU 305 RBCuZn-D
Cu48ZnNi9Ag 48 Bal 1 9 0,2 890-920 8,7 54
Anmerkungen Messing für Hochtemperaturlöten. RoHS-konform. Lieferbar als Stäbe, umhüllte Stäbe, Drähte und Ringe. Cu59ZnAg ist für vezinkten Stahl geeignet.

Fluxes

FLUX BR1 Messinglöten
FLUX LI2 Zum Löten mit Vaporizator. Mittel-hohe Konzentration
FLUX LI3 Zum Löten mit Vaporizator. Hohe Konzentration

Weichlote

Artikel Zusammensetzung % Schmelzbereich SOL-LIQ Normung
Sn Pb Ag Cu Sb Zn Cd °C ISO 9453 EN 29453

Alloys

SnPb60/40 60 40 183-190 No. 103 S-Sn60Pb40
Ag3,5Sn 96,5 3.5 221 No. 703 S-Sn97Ag3
Ag5Sn 95 5 221-235 No. 704
Anmerkungen Farbe Edelstahl ähnlich.

Fluxes

FLUX SN1 Allgemeine Verwendung
FLUX SN2 Für Edelstahl


ROHRKONSTRUKTIONEN

Tiziana

Hartlote für die Herstellung von:
Stahlmöbel, Fahrradrahmen, Motorfahrräder, usw.

Silberlegierungen

Artikel Zusammensetzung % Schmelzbereich SOL-LIQ Dichte Zugfestigkeit Normung
Ag Cu Zn Sn Si °C g/cm3 kg/mm2 ISO 17672 EN 1044 AWS A5.8

Alloys

Ag12 12 48 40 0,15 800-830 8,4 48 Ag 212 AG 207
Ag20 20 44 36 0,15 690-810 8,7 43 AG 206
Ag34Sn 34 36 27,5 2,5 630-730 9 48 Ag 134 AG 106
Ag40Sn 40 30 28 2 650-710 9,1 44 Ag 140 AG 105 BAg-28
Ag45Sn 45 27 25,5 2,5 640-680 9,2 43 Ag 145 AG 104 BAg-36
Ag55Sn 55 21 22 2 630-660 9,4 44 Ag 155 AG 103
Anmerkungen Cadmium-freie und RoHS-konform. Lieferbar als Stäbe, umhüllte Stäbe, Drähte und Ringe (Abmessungen auf Anfrage).

Fluxes

FLUX AG1 Allgemeine Verwendung
FLUX AG4 Allgemeine Verwendung – Sehr weit Temperaturbereich
FLUX AG7 Allgemeine Verwendung. Auch für Edelstahl

Kupferlegierungen

Artikel Zusammensetzung % Schmelzbereich SOL-LIQ Dichte Zugfestigkeit Brinell-Härte Normung
Cu Ag Mn Sn Si P °C g/cm3 kg/mm2 HB 2,5 DIN 1733 AWS A5.7

Alloys

Cu99,9 99.9 0.05 1080 8.9 22 50 ERCu
CuSn Bal x 0.8 x 1020-1050 8.9 22 60 SG-CuSn
CuAg Bal 1 x 1070-1080 8.9 20 60 SG-CuAg
CuSi3 Bal 1 3 965-1035 8.5 35 80 SG-CuSi3 ERCuSi-A

Messing

Artikel Zusammensetzung % Schmelzbereich SOL-LIQ Dichte Zugfestigkeit Normung
Cu Zn Ag Ni Mn Sn Si B Co P °C g/cm3 kg/mm2 ISO 17672 EN 1044 AWS A5.8

Alloys

Cu60Zn 60 Bal 0,3 875-895 8,4 40 Cu 470a CU 301
Cu59ZnSn 59 Bal 0,4 0,3 875-895 8,4 45 Cu 470 CU 302 RBCuZn-A
Cu59ZnSnMn 59 Bal 0,7 0,4 0,3 870-890 8,4 45 ~ Cu 471 ~ CU 304 ~ RBCuZn-C
Cu59ZnAg 59 Bal 1 0,1 0,1 0,1 860-890 8,4 45
Cu48ZnNi10 48 Bal 10 0,3 890-920 8,7 54 Cu 773 CU 305 RBCuZn-D
Cu48ZnNi9Ag 48 Bal 1 9 0,2 890-920 8,7 54
Anmerkungen Messing für Hochtemperaturlöten. RoHS-konform. Lieferbar als Stäbe, umhüllte Stäbe, Drähte und Ringe. Cu59ZnAg ist für vezinkten Stahl geeignet.

Fluxes

FLUX BR1 Messinglöten
FLUX LI1 Zum Löten mit Vaporizator. Mittel-Konzentration
FLUX LI2 Zum Löten mit Vaporizator. Mittel-hohe Konzentration
FLUX LI3 Zum Löten mit Vaporizator. Hohe Konzentration

Aluminium

Artikel Zusammensetzung % Normung
Al Si Mg Mn Zn Zr DIN 1732 AWS A5.10

Alloys

AlSi12 Bal 12 SG-AlSi12 4047
Anmerkungen Auch zum Löten.
AlMg4,5Mn Bal 0.2 4.5 0.5-1 SG-AlMg4,5Mn 5183
AlMg4,5MnZr Bal <0.4 4.5-5.2 0.7-1.1 <0.25 0.1-0.2 SG-AlMg4,5MnZr 5087
AlMg5 Bal 0.2 5 0.05-2 SG-AlMg5 5356


SOLARABSORBER

Tiziana

Hartlote für die Herstellung von:
Termische Solarabsorber.

Silberlegierungen

Artikel Zusammensetzung % Schmelzbereich SOL-LIQ Dichte Zugfestigkeit Normung
Ag Cu Zn Sn Si °C g/cm3 kg/mm2 ISO 17672 EN 1044 AWS A5.8

Alloys

Ag30Sn 30 36 32 2 665-755 8,8 48 Ag 130 AG 107
Ag34Sn 34 36 27,5 2,5 630-730 9 48 Ag 134 AG 106
Ag40Sn 40 30 28 2 650-710 9,1 44 Ag 140 AG 105 BAg-28
Ag45Sn 45 27 25,5 2,5 640-680 9,2 43 Ag 145 AG 104 BAg-36
Ag55Sn 55 21 22 2 630-660 9,4 44 Ag 155 AG 103
Anmerkungen RoHS-konform.

Fluxes

FLUX AG1 Allgemeine Verwendung
FLUX AG4 Allgemeine Verwendung – Sehr weit Temperaturbereich
FLUX AG7 Allgemeine Verwendung. Auch für Edelstahl

Kupferphosphorlegierungen

Artikel Zusammensetzung % Schmelzbereich SOL-LIQ Arbeitstemperatur Dichte Zugfestigkeit Normung
Ag Cu P Sn °C °C g/cm3 kg/mm2 ISO 17672 EN 1044 AWS A5.8

Alloys

CuP6 Bal. 6,3 710-890 760 8,1 56 CuP 179 CP 203
CuP7 Bal. 7,3 710-820 730 8,1 58 CuP 180 CP 202 BCuP-2
CuP8 Bal. 7,8 710-770 720 8 60 CuP 182 CP 201
CuP7Sn Bal. 7 7 650-700 700 8 60 CuP 386 CP 302 ~ BCuP-9
Ag2CuP 2 Bal. 6,5 645-825 740 8,1 55 CuP 279 CP 105
Ag5CuP 5 Bal. 6 645-815 710 8,2 55 CuP 281 CP 104 BCuP-3
Ag15CuP 15 Bal. 5 645-800 700 8,4 54 CuP 284 CP 102 BCuP-5
Anmerkungen RoHS-konform.
Für Kupfer-Kupfer und Kupfer-Messing Verbindungen.
Für Kupfer-Kupfer Verbindungen ist kein Flussmittel erforderlich.
Diese Legierungen sind nicht für Eisenmaterialien, Stahl, Nickellegierungen und schwefelhaltigen Atmosphären geeignet.
Silberlegierungen sind besonders geeignet für Verbindungen die widerstandsfähig gegen Vibrationen sein müssen.
Lieferbar als Stäbe, umhüllte Stäbe, Drähte und Ringe.

Fluxes

FLUX AG4 Allgemeine Verwendung – Sehr weit Temperaturbereich

Weichlote

Artikel Zusammensetzung % Schmelzbereich SOL-LIQ Normung
Sn Pb Ag Cu Sb Zn Cd °C ISO 9453 EN 29453

Alloys

SnCu97/3 97 3 227-310 No. 402 S-Sn97Cu3
Anmerkungen RoHS-konform.
Ag1,5SnPb 5 93,5 1,5 296-301
Ag5Sn 95 5 221-235 No. 704
Anmerkungen RoHS-konform.
SnPb50/50 50 50 183-215 No. 111 S-Pb50Sn50
SnPb40/60 40 60 183-235 No. 114 S-Pb60Sn40

Fluxes

FLUX SN1 Allgemeine Verwendung


ELEKTROMECHANISCHE KONSTRUKTIONEN

Tiziana

Hartlote für die Herstellung von:
Elektromechanischer Bau, Stromerzeuger, Stromwandler, Elektromotoren, Heizelementen, Lichtlote, Trennschalter und Relais, usw.

Silberlegierungen

Artikel Zusammensetzung % Schmelzbereich SOL-LIQ Dichte Zugfestigkeit Normung
Ag Cu Zn Sn Ni Si Mn In °C g/cm3 kg/mm2 ISO 17672 EN 1044 AWS A5.8

Alloys

Ag20 20 44 36 0,15 690-810 8,7 43 AG 206
Ag34Sn 34 36 27,5 2,5 630-730 9 48 Ag 134 AG 106
Ag40Ni 40 30 28 2 670-780 8,9 Ag 440 BAg-4
Ag40Ni/1 40 58 2 780-900 9,6 35
Anmerkungen RoHS-konform. Für Edelstahl in feuchten Umgebungen. Ag40Ni/1 ist auch für Ofenlöten geeignet.
Ag40Sn 40 30 28 2 650-710 9,1 44 Ag 140 AG 105 BAg-28
Ag44 45 30 26 675-735 9,1 51 Ag 244 AG 203
Ag45Sn 45 27 25,5 2,5 640-680 9,2 43 Ag 145 AG 104 BAg-36
Ag49MnNi 49 16 23 4,5 7,5 680-705 8,9 55 Ag 449 AG 502 BAg-22
Anmerkungen RoHS-konform. Für Hartmetall.
Ag49MnNi/1 TR 49 27,5 20,5 0,5 2,5 670-690 9,0
Anmerkungen RoHS-konform. Schichtfolienlot. Für Hartmetall. Mittel / groß Hartmetallstücke.
Ag50Ni 50 20 28 2 660-705 9,0 45 Ag 450 BAg-24
Anmerkungen RoHS-konform. Für Edelstahl in feuchten Umgebungen.
Ag55Sn 55 21 22 2 630-660 9,4 44 Ag 155 AG 103
Ag56Sn 56 22 17 5 620-655 9,4 48 Ag 156 AG 102 BAg-7
Ag60 60 26 14 695-730 9,5 45 AG 202
Ag60Sn 60 23 14 3 620-685 9,6 48 AG 101
Ag72 72 28 780-780 10 35 Ag 272 AG 401 BAg-8
Anmerkungen RoHS-konform. Diese Legierungen sind für Ofenlöten geeignet. Ag60Sn/1 ist auch für Edelstahl in feuchten Umgebungen geeignet.

Fluxes

FLUX AG1 Allgemeine Verwendung
FLUX AG4 Allgemeine Verwendung – Sehr weit Temperaturbereich
FLUX AG7 Allgemeine Verwendung. Auch für Edelstahl
FLUX AG8 Für Edelstahl und Hartmetall – Braune Paste

Kupferphosphorlegierungen

Artikel Zusammensetzung % Schmelzbereich SOL-LIQ Arbeitstemperatur Dichte Zugfestigkeit Normung
Ag Cu P Sn °C °C g/cm3 kg/mm2 ISO 17672 EN 1044 AWS A5.8

Alloys

CuP7Sn Bal. 7 7 650-700 700 8 60 CuP 386 CP 302 ~ BCuP-9
Ag2CuP 2 Bal. 6,5 645-825 740 8,1 55 CuP 279 CP 105
Ag5CuP 5 Bal. 6 645-815 710 8,2 55 CuP 281 CP 104 BCuP-3
Anmerkungen RoHS-konform. Für Kupfer-Kupfer und Kupfer-Messing Verbindungen.

Fluxes

FLUX AG4 Allgemeine Verwendung – Sehr weit Temperaturbereich

Weichlote

Artikel Zusammensetzung % Schmelzbereich SOL-LIQ Normung
Sn Pb Ag Cu Sb Zn Cd °C ISO 9453 EN 29453

Alloys

Ag1,5SnPb 5 93,5 1,5 296-301
Sn60Pb38Cu2 60 38 2 183-190 No. 161 S-Sn60Pb38Cu2

Fluxes

FLUX SN6 Für Elektromechanik


MEß -UND REGELUNGSGERÄTE

Tiziana

Hartlote für die Herstellung von:
Maßgeräte, Thermostate, Druckschalter, Druckmessgeräte, Hygrometer, usw.

Kupferphosphorlegierungen

Artikel Zusammensetzung % Schmelzbereich SOL-LIQ Arbeitstemperatur Dichte Zugfestigkeit Normung
Ag Cu P Sn °C °C g/cm3 kg/mm2 ISO 17672 EN 1044 AWS A5.8

Alloys

CuP7Sn Bal. 7 7 650-700 700 8 60 CuP 386 CP 302 ~ BCuP-9
Ag5CuP 5 Bal. 6 645-815 710 8,2 55 CuP 281 CP 104 BCuP-3
Ag15CuP 15 Bal. 5 645-800 700 8,4 54 CuP 284 CP 102 BCuP-5
Anmerkungen RoHS-konform. Für Kupfer-Kupfer und Kupfer-Messing Verbindung.

Fluxes

FLUX AG4 Allgemeine Verwendung – Sehr weit Temperaturbereich

Silberlegierungen

Artikel Zusammensetzung % Schmelzbereich SOL-LIQ Dichte Zugfestigkeit Normung
Ag Cu Zn Ni Mn Si Sn In °C g/cm3 kg/mm2 ISO 17672 EN 1044 AWS A5.8

Alloys

Ag40Ni 40 30 28 2 670-780 8,9 Ag 440 BAg-4
Ag40Ni/1 40 58 2 780-900 9,6 35
Anmerkungen RoHS-konform. Für Edelstahl in feuchten Umgebungen. Ag40Ni/1 ist auch für Ofenlöten geeignet.
Ag40Sn 40 30 28 2 650-710 9,1 44 Ag 140 AG 105 BAg-28
Ag44 45 30 26 675-735 9,1 51 Ag 244 AG 203
Ag45Sn 45 27 25,5 2,5 640-680 9,2 43 Ag 145 AG 104 BAg-36
Ag50Ni 50 20 28 2 660-705 9,0 45 Ag 450 BAg-24
Anmerkungen RoHS-konform. Für Edelstahl in feuchten Umgebungen.
Ag55Sn 55 21 22 2 630-660 9,4 44 Ag 155 AG 103
Ag56Sn 56 22 17 5 620-655 9,4 48 Ag 156 AG 102 BAg-7
Ag60 60 26 14 695-730 9,5 45 AG 202
Ag60Sn 60 23 14 3 620-685 9,6 48 AG 101
Ag72 72 28 780-780 10 35 Ag 272 AG 401 BAg-8
Anmerkungen RoHS-konform. Diese Legierungen sind für Ofenlöten geeignet. Ag60Sn/1 ist auch für Edelstahl in feuchten Umgebungen geeignet.

Fluxes

FLUX AG1 Allgemeine Verwendung
FLUX AG4 Allgemeine Verwendung – Sehr weit Temperaturbereich
FLUX AG7 Allgemeine Verwendung. Auch für Edelstahl

Weichlote

Artikel Zusammensetzung % Schmelzbereich SOL-LIQ Normung
Sn Pb Ag Cu Sb Zn Cd °C ISO 9453 EN 29453

Alloys

SnPb40/60 40 60 183-235 No. 114 S-Pb60Sn40
SnPb60/40 60 40 183-190 No. 103 S-Sn60Pb40
SnCu97/3 97 3 227-310 No. 402 S-Sn97Cu3
Ag3,5Sn 96,5 3.5 221 No. 703 S-Sn97Ag3
Ag5Sn 95 5 221-235 No. 704
Ag10Sn 90 10 221-300
Anmerkungen RoHS-konform.

Fluxes

FLUX SN1 Allgemeine Verwendung
FLUX SN2 Für Edelstahl


KÄLTE UND KLIMA-TECHNIK: INSTALLATION

Tiziana

Hartlote für die Installation und die Herstellung von:
Klimaanlagen, Heizungsanlagen, Wasser-Gas-und Dampf Verteilungsanlagen, Bodenheizung, Solarabsorber, usw.

NEUE PRODUKTE: bitte fragen Sie uns nach der neu eingeführten PLUS-Version von Kupfer-Phosphor-Legierungen für Kupfer Löten!

Kupfer-Phosphor-(Silber)-Hartlote

Artikel Zusammensetzung % Schmelzbereich SOL-LIQ Arbeitstemperatur Dichte Zugfestigkeit Normung
Ag Cu P Sn °C °C g/cm3 kg/mm2 ISO 17672 EN 1044 AWS A5.8

Alloys

CuP6 Bal. 6,3 710-890 760 8,1 56 CuP 179 CP 203
CuP7 Bal. 7,3 710-820 730 8,1 58 CuP 180 CP 202 BCuP-2
CuP8 Bal. 7,8 710-770 720 8 60 CuP 182 CP 201
CuP7Sn Bal. 7 7 650-700 700 8 60 CuP 386 CP 302 ~ BCuP-9
Ag2CuP 2 Bal. 6,5 645-825 740 8,1 55 CuP 279 CP 105
Ag5CuP 5 Bal. 6 645-815 710 8,2 55 CuP 281 CP 104 BCuP-3
Ag15CuP 15 Bal. 5 645-800 700 8,4 54 CuP 284 CP 102 BCuP-5
Anmerkungen RoHS-konform. Für Kupfer-Kupfer und Kupfer-Messing Verbindungen. Für Kupfer-Kupfer Verbindungen ist kein Flussmittel erforderlich.
Diese Legierungen sind nicht für Eisenmaterialien, Stahl, Nickellegierungen und schwefelhaltigen Atmosphären geeignet.
Silberlegierungen sind besonders geeignet für Verbindungen die widerstandsfähig gegen Vibrationen sein müssen.
Diese Legierungen sind lieferbar als Stäbe, umhüllte Stäbe, Drähte und Ringe.

Fluxes

FLUX AG4 Allgemeine Verwendung – Sehr weit Temperaturbereich

Silberlote

Artikel Zusammensetzung % Schmelzbereich SOL-LIQ Dichte Zugfestigkeit Normung
Ag Cu Zn Sn Ni Si Mn In °C g/cm3 kg/mm2 ISO 17672 EN 1044 AWS A5.8

Alloys

Ag12 12 48 40 0,15 800-830 8,4 48 Ag 212 AG 207
Ag20 20 44 36 0,15 690-810 8,7 43 AG 206
Ag30Sn 30 36 32 2 665-755 8,8 48 Ag 130 AG 107
Ag34Sn 34 36 27,5 2,5 630-730 9 48 Ag 134 AG 106
Ag35 35 32 33 685-755 9 48 Ag 235 BAg-35
Ag40Sn 40 30 28 2 650-710 9,1 44 Ag 140 AG 105 BAg-28
Ag45Sn 45 27 25,5 2,5 640-680 9,2 43 Ag 145 AG 104 BAg-36
Ag55Sn 55 21 22 2 630-660 9,4 44 Ag 155 AG 103
Ag56Sn 56 22 17 5 620-655 9,4 48 Ag 156 AG 102 BAg-7
Anmerkungen Cadmiumfreie und RoHS-konform.
Diese Legierungen sind für Eisen-und nichteisenmaterialien (Kupfer, Messing, Bronze, Stahl, Edelstahl, Nickellegierungen) geeignet außer Aluminium und Magnesium
Lieferbar als Stäbe, umhüllte Stäbe, Drähte und Ringe (Abmessungen auf Anfrage).
Ag60Sn/1 60 30 10 600-730 9,8 Ag 160 AG 402 BAg-18
Anmerkungen Für Edelstahl in feuchten Umgebungen.
Ag72Zn 72 28 710-730 8,4 44
Ag85Mn 85 15 960-970 10 Ag 485 AG 501 BAg-23
Anmerkungen Legierungen ohne Kupfer, ammoniakbeständig. Ag85Mn ist für Edelstahl in feutchten Umgebungen geeignet.

Fluxes

FLUX AG1 Allgemeine Verwendung
FLUX AG4 Allgemeine Verwendung – Sehr weit Temperaturbereich
FLUX AG7 Allgemeine Verwendung. Auch für Edelstahl

Weichlote

Artikel Zusammensetzung % Schmelzbereich SOL-LIQ Normung
Sn Pb Ag Cu Sb Zn Cd °C ISO 9453 EN 29453

Alloys

SnCu97/3 97 3 227-310 No. 402 S-Sn97Cu3
Ag3,5Sn 96,5 3.5 221 No. 703 S-Sn97Ag3
Ag5Sn 95 5 221-235 No. 704
Anmerkungen Blei-frei, RoHS-konform. Geeignet für Trinkwasser und Lebensmittel.

Fluxes

FLUX SN1 Allgemeine Verwendung

Aluminiumlote und Zink-Aluminiumlote

Artikel Zusammensetzung % Schmelzbereich SOL-LIQ Normung
Al Si Mg Mn Zn °C DIN 1732 ISO 17672 AWS A5.10 EN 1044 AWS A5.8

Alloys

AlSi12 Bal 12 SG-AlSi12 4047
Anmerkungen Aluminiumlöten.
AlZn78 22 78 441-471
AlZn98 2 98 380-405
Anmerkungen Für Kupfer-Aluminium und Messing-Aluminium Vebindungen. Auch lieferbar als flussmittelgefüllte Stäbe und Drähte (nicht-korrosives Flussmittel).

Fluxes

FLUX AL1/d Toxisches Flussmittel für Flammlöten
FLUX AL6 Nicht toxisches Flussmittel für Zink-Aluminiumlegierungen